OD(mm): 10, 10.9, 12, 12.7, 13, 13.95, 14, 16, etc. Thickness(mm): 1.0, 1.2, 1.5, 2.0, etc. Length(mm): 50-12000. Standard: JIS G 3445, DIN 17100, DIN 17102, EN10268, EN10338, GB/T 11253, GB/T 1591, etc. Grade: STKM12B, STKM13A, STKM13B, ST37-2G, ST52-3G, HC340LA, HC420LA, HC480LA, HC500LA, HCT590X, HCT780X, HCT980X, Q235B, Q355B, etc. For requirements out of the established specification range, we can arrange the trial production after further discussion and agreement.
Product Features
Automotive headrests serve both as comfort accessories and safety devices in automobiles. During rear-end collisions, inertia causes the human body to lurch backward, and the pressure resulting from the automobile's sudden acceleration or deceleration intensely focuses on the vulnerable neck and head area. The headrest plays a crucial buffering role at this situation, mitigating the impact, protecting the head and minimizing potential injury.
Parameter
Chemical Composition (Heat Analysis) (%)
Grade |
C |
Si |
Mn |
P |
S |
Alt |
Ti |
Nb |
HC340LA |
≤0.1 |
≤0.5 |
≤1.1 |
≤0.025 |
≤0.025 |
≥0.015 |
≤0.15 |
≤0.09 |
HC380LA |
≤0.1 |
≤0.5 |
≤1.6 |
≤0.025 |
≤0.025 |
≥0.015 |
≤0.15 |
≤0.09 |
HC420LA |
≤0.1 |
≤0.5 |
≤1.6 |
≤0.025 |
≤0.025 |
≥0.015 |
≤0.15 |
≤0.09 |
Mechanical Properties
Grade |
Status |
Rpl (MPa) |
Rm (MPa) |
A L0=80mm(%) |
HC340LA |
Cold Rolled |
340-420 |
410-540 |
≥21 |
HC380LA |
Cold Rolled |
380-480 |
440-560 |
≥19 |
HC420LA |
Cold Rolled |
420-520 |
470-590 |
≥17 |
Tolerances
Production standards and tube tolerance standards base on EN10305-3, JIS-G 3445, GB/T 13793, etc. And the tolerance could be customized according to customer’s requirement.
1.Selecting high-quality carbon steel as the raw material, which boasts favorable mechanical properties, including strength and toughness and demonstrates stable performance during bending, punching and other processing procedures.
2.CBIES uses advanced high-frequency welding technology to ensure the consistent quality of weld joints, effectively minimizing welding defects. This approach enhances the strength and fatigue life of welded areas, thereby guaranteeing the safety of the product during usage.
3.During the welding process, strict control is exerted over welding parameters such as current, voltage and speed to ensure the integrity of the weld quality. Additionally, post-weld treatments are implemented, including online cleaning of the weld seam and real-time inspection for flaws, to confirm there is on defect such as cracks, incomplete penetration and slag inclusion in the welded areas.